Polymer Property : CTE, linear = 4.68 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 4.68 µm/m-°C

@Temperature 20.0 °C
2.60 µin/in-°F

@Temperature 68.0 °F
SGL Carbon Group EK 204 Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
CTE, linear 4.68 µm/m-°C

@Temperature 20.0 °C
2.60 µin/in-°F

@Temperature 68.0 °F
SGL Carbon Group EK 3245 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
CTE, linear 4.68 µm/m-°C

@Temperature 20.0 °C
2.60 µin/in-°F

@Temperature 68.0 °F
Cotronics Resbond™ 919 High Temperature Ceramic Adhesive, High Resistance
CTE, linear 4.68 µm/m-°C

@Temperature 20.0 °C
2.60 µin/in-°F

@Temperature 68.0 °F
Blasch Ceramics NITRON Nitride bonded SiC
Features:Properties suit many severe operating conditionsGood wear and abrasionResists wetting by non-ferrous metalsHigh mechanical strengthExcellent Thermal shock resistance