Thermal Properties Metric English Comments
CTE, linear 40.3 µm/m-°C

@Temperature 20.0 °C
22.4 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Gharda Chemicals Gafone S 1500 Polysulfone (PS)  (discontinued **)
Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec..