Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 21.0 - 77.0 µm/m-°C | 11.7 - 42.8 µin/in-°F | Average value: 39.7 µm/m-°C Grade Count:3 |
Overview of materials for PEKK, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Unreinforced". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
CTE, linear | 39.6 - 77.0 µm/m-°C | 22.0 - 42.8 µin/in-°F | Average value: 58.0 µm/m-°C Grade Count:5 |
Overview of materials for Polycarbonate/ABS Alloy, Antistat/Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Antistat/Conductive". Each property range of values reported is minimum and max.. |