Polymer Property : CTE, linear = 450 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 810 µm/m-°C

@Temperature 20.0 °C
450 µin/in-°F

@Temperature 68.0 °F
Fluorosilicone Rubber (FMQ, FVMQ, FSi)
Resists ozone and oxidizing chemicals, alkali, aromatic chlorinated solvents. Affected by brake fluid, ketones, and hydrazine.