Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 88.2 µm/m-°C @Temperature -40.0 - 149 °C |
49.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Fluorosint® HPV Mica-filled PTFE (ASTM Product Data Sheet) |
|||
CTE, linear | 88.2 µm/m-°C @Temperature -40.0 - 149 °C |
49.0 µin/in-°F @Temperature -40.0 - 300 °F |
ASTM E831 |
Quadrant EPP Nylatron® 703 XL Cast, Wear Resistant, Zero 'Stick-Slip' (ASTM Product Data Sheet) |
|||
CTE, linear | 88.2 µm/m-°C @Temperature 20.0 °C |
49.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Stratasys® ABSplus ABSplus is up to 40 percent stronger than standard ABS material and is an ideal material for conceptual prototyping through design verification through direct digital manufacturing. The marriage of .. |
|||
CTE, linear | 88.2 µm/m-°C @Temperature 20.0 °C |
49.0 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Stratasys® ABS-M30 ABS-M30 is 25-70 percent stronger than standard Stratasys ABS and is an ideal material for conceptual prototyping, design verification, and direct digital manufacturing. ABS-M30 has greater tensile,.. |
|||
CTE, linear | 88.2 µm/m-°C @Temperature -40.0 - 37.8 °C |
49.0 µin/in-°F @Temperature -40.0 - 100 °F |
ASTM E831 |
Stratasys® ABS-M30i ABS-M30i is a high strength material well suited for the medical, pharmaceutical
and food packaging industries. Parts manufactured with ABS-M30i material
are biocompatible (ISO 10993 certified) an.. |
|||
CTE, linear | 88.2 µm/m-°C @Temperature 20.0 °C |
49.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Pomalux® CN-SS Acetal Copolymer (conductive) Stainless-steel-fiber-filled, non-sloughing, dimensionally stable material HDT @ 264 psi of 225F. This material has relatively high chemical resistance, is extremely strong and stiff, and is an exc.. |