Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 9.50 µm/m-°C @Temperature 20.0 °C |
5.28 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech Ceraflex 8Y Thin Zirconia Ceramic Oxygen Ion Conductor, Yttria Stabilized Data provided by the supplier, MarkeTech International.8 mole% Y2O3 (13.8 wt%). CERAFLEX is a sintered and fully dense zirconia ceramic material that is formed into extremely thin sheets, that are .. |
|||
CTE, linear | 9.50 - 10.2 µm/m-°C @Temperature 20.0 - 100 °C |
5.28 - 5.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
MarkeTech W75Cu Tungsten/Copper Heat Sink Material WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c.. |
|||
CTE, linear | 9.50 µm/m-°C | 5.28 µin/in-°F | at Set Pt. |
Ferro EG 2927 Metal Sealing Glass Type: Sr-B-Al Typical Powder Form: VSD Typical Application: Comp. - Battery Ferro Metal Sealing glasses are formulated for sealing a wide range of metal packages and parts, including matched .. |
|||
CTE, linear | 9.50 - 11.0 µm/m-°C @Temperature 20.0 - 100 °C |
5.28 - 6.11 µin/in-°F @Temperature 68.0 - 212 °F |
|
Goodfellow Havar® High-Strength Non-Magnetic Cobalt-Base Alloy Co42.5/Cr20/Ni13/Fe/W/Mo/MnInformation provided by Goodfellow. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 20.0 °C |
5.28 µin/in-°F @Temperature 68.0 °F |
|
Goodfellow Permendur 49® Cobalt Iron Magnetic Alloy Information provided by Goodfellow. |
|||
CTE, linear | 9.50 µm/m-°C @Temperature 25.0 - 1000 °C |
5.28 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
CoorsTek Porcelain Information provided by CoorsTek. |
|||
CTE, linear | 9.50 µm/m-°C | 5.28 µin/in-°F | at Set Pt. (Fired Thermal Expansion) |
Ferro CF 7572 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci.. |