Polymer Property : CTE, linear = 59.0 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 35.0 - 59.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
19.4 - 32.8 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
SABIC Innovative Plastics Lexan® LC108 PC (Asia Pacific)
Polycarbonate base, 8% carbon fiber reinforced, FR