Polymer Property : CTE, linear = 6.33 µm/m-°C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 6.33 µm/m-°C

@Temperature 1000 °C
3.52 µin/in-°F

@Temperature 1830 °F
Chosun Refractories CRZG-L30 Shroud Nozzle