Polymer Property : CTE, linear = 6.60 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 11.9 µm/m-°C

@Temperature 20.0 °C
6.60 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Owens Corning Glass Fiber Reinforced Polyester BMC (Injection), 22 wt.% glass
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u..
CTE, linear 11.9 µm/m-°C

@Temperature 20.0 °C
6.60 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Owens Corning Glass Fiber Reinforced Polyester SMC (Compression), 22 wt.% glass
Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u..
CTE, linear 11.9 µm/m-°C

@Temperature 37.8 - 538 °C
6.60 µin/in-°F

@Temperature 100 - 1000 °F
Meehanite GC-40 Flake Graphite Cast Iron
Type GC-40 combines good strength with low coefficient of friction and self lubricating properties. It is easily machinable with a fine, dense, close grain structure. Recommended for heavy brake d..
CTE, linear 11.9 µm/m-°C

@Temperature 20.0 - 649 °C
6.60 µin/in-°F

@Temperature 68.0 - 1200 °F
Eagle Brass 430 Ferritic Stainless Steel, 1/2 Hardened
Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro..
CTE, linear 11.9 µm/m-°C

@Temperature 20.0 - 649 °C
6.60 µin/in-°F

@Temperature 68.0 - 1200 °F
Eagle Brass 430 Ferritic Stainless Steel, 1/4 Hardened
Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro..
CTE, linear 11.9 µm/m-°C

@Temperature 20.0 - 649 °C
6.60 µin/in-°F

@Temperature 68.0 - 1200 °F
Eagle Brass 430 Ferritic Stainless Steel, Annealed
Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro..
CTE, linear 11.9 µm/m-°C

@Temperature 20.0 - 649 °C
6.60 µin/in-°F

@Temperature 68.0 - 1200 °F
Eagle Brass 430 Ferritic Stainless Steel, Full Hardened
Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro..
CTE, linear 11.9 µm/m-°C

@Temperature 20.0 - 649 °C
6.60 µin/in-°F

@Temperature 68.0 - 1200 °F
Schmolz + Bickenbach IMRE™ Stainless Steel Bar
Description: Ugine IMRE™ is a chromium stainless steel with improved magnetic properties used in solenoid valves. IMRE™ is at 18% chromium ferritic stainless steel with 2% Mo designed to withstand..