Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.90 µm/m-°C | 4.39 µin/in-°F | |
Poco Graphite AXF-5Q Industrial Grade Graphite POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr.. |
|||
CTE, linear | 7.90 µm/m-°C | 4.39 µin/in-°F | |
Poco Graphite TRA Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
CTE, linear | 7.90 - 121 µm/m-°C | 4.39 - 67.2 µin/in-°F | Average value: 92.5 µm/m-°C Grade Count:43 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
CTE, linear | 7.90 µm/m-°C | 4.39 µin/in-°F | at Set Pt. (Fired Thermal Expansion) |
Ferro EG 2012 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
CTE, linear | 7.90 µm/m-°C @Temperature 20.0 - 650 °C |
4.39 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Du-Co Ceramics DC-265-L-6 Alumina, 96% Al2O3 Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
CTE, linear | 7.90 µm/m-°C | 4.39 µin/in-°F | DIN EN 821-1 |
CeramTec 614/698 Alumina, 96% 614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink. |
|||
CTE, linear | 7.90 µm/m-°C @Temperature 27.0 °C |
4.39 µin/in-°F @Temperature 80.6 °F |
|
Mateck Window Grade Zinc Selenide, ZnSe Optical Crystals |