Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 80.0 - 121 µm/m-°C | 44.4 - 67.2 µin/in-°F | Average value: 103 µm/m-°C Grade Count:9 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m.. |
|||
CTE, linear | 7.90 - 121 µm/m-°C | 4.39 - 67.2 µin/in-°F | Average value: 92.5 µm/m-°C Grade Count:43 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
CTE, linear | 101 - 121 µm/m-°C @Temperature 20.0 °C |
56.0 - 67.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
CPC - Vycom FLAMETEC™ KYTEC® PVDF Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e.. |