Polymer Property : CTE, linear = 73.3 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 132 µm/m-°C

@Temperature -50.0 - 100 °C
73.3 µin/in-°F

@Temperature -58.0 - 212 °F
Sorbothane Polyurethane Damping Material, 30 Durometer
Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the m..
CTE, linear 132 µm/m-°C

@Temperature -50.0 - 100 °C
73.3 µin/in-°F

@Temperature -58.0 - 212 °F
Sorbothane Polyurethane Damping Material, 50 Durometer
Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the m..
CTE, linear 132 µm/m-°C
73.3 µin/in-°F
Above Tg
Epoxy Technology EPO-TEK® 323LP Epoxy
Material Description: Longer pot life version of EPO-TEK® 353ND designed for semiconductor, hybrid, fiber-optic, hard-disk drive and medical applications.Information Provided by Epoxy Technology
CTE, linear 132 µm/m-°C
73.3 µin/in-°F
Below Tg
3M Scotch-Weld™ DP8010NS Structural Adhesive
3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop..
CTE, linear 132 µm/m-°C

@Temperature -50.0 - 100 °C
73.3 µin/in-°F

@Temperature -58.0 - 212 °F
Sorbothane Polyurethane Damping Material, 70 Durometer
Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the mat..