Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.90 µm/m-°C | 4.94 µin/in-°F | at Set Pt. |
Ferro CF 7575 Display Device Glass Type: Pb-Zn-B (Composite) Typical Powder Form: VSD Typical Application: Seal (Devitrified) Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for herm.. |
|||
CTE, linear | 8.90 µm/m-°C | 4.94 µin/in-°F | at Set Pt. (Fired Thermal Expansion) |
Ferro EG 2020 Low-Temperature Sealing VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp.. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 20.0 - 300 °C |
4.94 µin/in-°F @Temperature 68.0 - 572 °F |
ISO 7991 |
Schott Glass 8516 Sealing Glass Sealing glass for Fe-Ni alloys, high IR-absorbing, lead-free, of poor evaporation Reed switches The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10.. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 20.0 - 300 °C |
4.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott S8008G Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 20.0 - 300 °C |
4.94 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott S8807 Contrast Enhancement Filter Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 20.0 °C |
4.94 µin/in-°F @Temperature 68.0 °F |
|
Sapco 99.7% Aluminum Oxide Information provided by Sapco. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 20.0 °C |
4.94 µin/in-°F @Temperature 68.0 °F |
|
Sapco 99.9% Aluminum Oxide Information provided by Sapco. |
|||
CTE, linear | 8.90 µm/m-°C @Temperature 0.000 - 300 °C |
4.94 µin/in-°F @Temperature 32.0 - 572 °F |
|
Corning 9010 Alkali Barium Crushed Glass Used for sealing and other applications.Information provided by Corning Incorporated. |
|||
CTE, linear | 8.90 µm/m-°C | 4.94 µin/in-°F | at Set Pt. (Fired Thermal Expansion) |
Ferro CF 7575 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci.. |