Ferro CF 7575 Display Device

Category Ceramic , Glass
Manufacturer Ferro Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ferro CF 7575 Display Device.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass Type: Pb-Zn-B (Composite) Typical Powder Form: VSD Typical Application: Seal (Devitrified) Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and passivation of soda lime glass packages, including plasma display panels and tubes.Information provided by Ferro Corporation
Physical Properties Metric English Comments
Density 6.20 g/cc
0.224 lb/in³
Particle Size >= 16 µm
>= 16 µm
50% of particles
<= 105 µm
<= 105 µm
Thermal Properties Metric English Comments
CTE, linear 8.90 µm/m-°C
4.94 µin/in-°F
at Set Pt.
8.30 µm/m-°C

@Temperature 260 °C
4.61 µin/in-°F

@Temperature 500 °F
Softening Point 370 °C
698 °F
Transformation Temperature 300 °C
572 °F
Processing Properties Metric English Comments
Processing Temperature 460 °C
860 °F
Typical Firing Temperature; Typical Firing Time: 60 min.