Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 75.6 - 166 µm/m-°C | 42.0 - 92.2 µin/in-°F | Average value: 117 µm/m-°C Grade Count:6 |
Overview of materials for ABS/PVC Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/PVC Alloy". Each property range of values reported is minimum and maximum values of appropriate MatW.. |