Thermal Properties Metric English Comments
Thermal Conductivity 0.0376 W/m-K
0.261 BTU-in/hr-ft²-°F
0.032 g/cc density
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer
ARCEL is a high-performance, moldable foam resin consisting of 70% polystyrene (PS) and 30% polyethylene (PE). ARCEL provides toughness, flexibility and durability in a lightweight foam.The strength..