Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0376 W/m-K | 0.261 BTU-in/hr-ft²-°F | 0.032 g/cc density |
NOVA Chemicals Arcel 730 70% PS/30% PE Interpolymer ARCEL is a high-performance, moldable foam resin consisting of 70% polystyrene (PS) and 30% polyethylene (PE). ARCEL provides toughness, flexibility and durability in a lightweight foam.The strength.. |