Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0448 W/m-K | 0.310 BTU-in/hr-ft²-°F | ASTM D3575, Suffix V |
Dow STRANDFOAM™ EA 1000 Polypropylene Foam STRANDFOAM™ EA 1000 Energy Absorbing polypropylene foam is a strong, low-density, closed-cell foam. It is suited as a component material in products requiring a shock and energy absorbing or vibra.. |