Thermal Properties Metric English Comments
Thermal Conductivity 0.0690 W/m-K
0.479 BTU-in/hr-ft²-°F
at ambient temperature
Skamol Group Exfoliated/Loose Vermiculite Loose Vermiculite
SKAMOL exfoliated vermiculite has the following characteristics: Max. service temperature: Up to 1200°C (2192°F)Good thermal insulating propertiesLow densityLow heat capacityAbsorbing and free..
Thermal Conductivity 0.0690 W/m-K
0.479 BTU-in/hr-ft²-°F
3M 4014 Damping Aluminum Foam Sheet
3M™ Damping Aluminum Foam Sheet 4014 is an open-cell polyurethane foam with an aluminum constraining layer on one side and a pressure sensitive adhesive on the opposite side to facilitate attachmen..