Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.134 W/m-K | 0.930 BTU-in/hr-ft²-°F | |
Americas Styrenics Styron® XL-8023VC High Impact Polystyrene
(discontinued **) STYRON® XL-8023 VC high impact polystyrene is designed to provide molders of VCR cassettes with the impact and gloss they require, at economics and processability highly advantaged over ABS resins... |
|||
Thermal Conductivity | 0.134 W/m-K | 0.930 BTU-in/hr-ft²-°F | |
Styron Magnum™ 9030 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Thermal Conductivity | 0.134 W/m-K | 0.930 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® DP 9659DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro.. |
|||
Thermal Conductivity | 0.134 W/m-K | 0.930 BTU-in/hr-ft²-°F | Melt |
Covestro Desmopan® DP 9662DU Polyurethane Extrusion- and injection molding gradewith special UV stabilizerstransparent up to 6 mm wall thicknessvery good hydrolysis and microbial resistanceApplicationSki boot shellsHosesnon-reinforcedPrepro.. |
|||
Thermal Conductivity | 0.134 W/m-K | 0.930 BTU-in/hr-ft²-°F | |
Dow Corning XIAMETER® PMCPPMX-200 10CS Silicone Fluid Is chemically equivalent to DOW CORNING® 200 FLUID 10CS. 100% active, 10 cSt, polydimethylsiloxane polymer.Information provided by Dow Corning |