Polymer Property : Thermal Conductivity = 0.225 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.225 W/m-K
1.56 BTU-in/hr-ft²-°F
ASTM C177
Plaskolite Vivak PETG Sheet
VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details...
Thermal Conductivity 0.225 W/m-K
1.56 BTU-in/hr-ft²-°F
ASTM F433
Quadrant EPP Duratron® PEI U2300 Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet)
Thermal Conductivity 0.225 - 0.259 W/m-K
1.56 - 1.80 BTU-in/hr-ft²-°F
Average value: 0.250 W/m-K Grade Count:8
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E..
Thermal Conductivity 0.225 W/m-K
1.56 BTU-in/hr-ft²-°F
ASTM D2214
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI
TECAPEI™ is an amorphous thermoplastic polyetherimide (PEI) made from Sabic Innovative Plastics' Ultem® 1000 and 2000 series resins. The unreinforced 1000 series materials are translucent amber in..