Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0385 W/m-K | 0.267 BTU-in/hr-ft²-°F | 12 g/l; EN 12667 |
Jackon JACKOCELL® R211 Expanded Polystyrene Construction and Block Molding High quality processingHigh strengthLow wasteFast moulding cycles |