Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.272 W/m-K | 1.89 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NX9270 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.272 W/m-K | 1.89 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NX9294 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.272 W/m-K | 1.89 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NX9300 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.272 W/m-K | 1.89 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NX9320 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.272 W/m-K | 1.89 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NY9208 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.272 W/m-K | 1.89 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NY9217 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.272 W/m-K | 1.89 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NY9220 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.272 W/m-K | 1.89 BTU-in/hr-ft²-°F | ASTM E1225 |
Park Electrochemical Nelco® NY9233 PTFE Laminate, Woven-Glass Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
Thermal Conductivity | 0.272 W/m-K | 1.88 BTU-in/hr-ft²-°F | |
Cytec EN-2521 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
Thermal Conductivity | 0.272 W/m-K | 1.88 BTU-in/hr-ft²-°F | |
Cytec EN-2532 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |