Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.198 - 0.288 W/m-K | 1.37 - 2.00 BTU-in/hr-ft²-°F | Average value: 0.230 W/m-K Grade Count:13 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Thermal Conductivity | 0.231 - 0.288 W/m-K | 1.60 - 2.00 BTU-in/hr-ft²-°F | Average value: 0.269 W/m-K Grade Count:3 |
Overview of materials for Polypropylene with 40% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Calcium Carbonate (CaCO3) Filler". Specific grades with primary filler content be.. |