Thermal Properties Metric English Comments
Thermal Conductivity 0.198 - 0.288 W/m-K
1.37 - 2.00 BTU-in/hr-ft²-°F
Average value: 0.230 W/m-K Grade Count:13
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Thermal Conductivity 0.197 W/m-K
1.37 BTU-in/hr-ft²-°F
Melt
Covestro Makroblend® KU 2-7609 Polycarbonate + PBT, Mineral Filled Impact Grade
ISO 7792-1-PC/PBT,MHPR,-030,MD20(PC+PBT)-blendsimpact modifiedInjection molding grade20% mineral filledPreprocessingMax. Water content
Thermal Conductivity 0.198 W/m-K
1.37 BTU-in/hr-ft²-°F
Melt
Covestro Makrolon® 1095 Polycarbonate, 15% Glass Filled
ISO 7391-PC,MR,(,,)-09-9,GF15Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min15 % Glass fiber reinforcedHigh viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CExtrusionAvailable ..
Thermal Conductivity 0.198 W/m-K
1.37 BTU-in/hr-ft²-°F
Melt
Covestro Makrolon® GF8002* Polycarbonate, 15% Glass Filled
ISO 7391-PC,MR,(,,)-09-9,GF15Formerly Makrolon DP1-1882MVR (300 °C/1.2 kg) 9.5 cm3/10 min15 % Glass fiber reinforcedMedium viscosityEasy releaseInjection molding - Melt temperature 310 - 330 °CAva..
Thermal Conductivity 0.197 W/m-K
1.37 BTU-in/hr-ft²-°F
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..