Polymer Property : Thermal Conductivity = 0.329 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.329 W/m-K
2.28 BTU-in/hr-ft²-°F
Melt
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned)
Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio..
Thermal Conductivity 0.329 W/m-K
2.28 BTU-in/hr-ft²-°F
Melt
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry)
Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio..