Polymer Property : Thermal Conductivity = 0.334 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.334 W/m-K
2.32 BTU-in/hr-ft²-°F
3M Scotch-Weld™ 3501 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 3501 B/A Gray is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume ar..
Thermal Conductivity 0.334 W/m-K
2.32 BTU-in/hr-ft²-°F
3M Scotch-Weld™ DP 3501 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP 3501 is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume are easi..