Material Notes:
3M™ Scotch-Weld™ Epoxy Adhesive DP 3501 is a rapid room temperature curing, two-part epoxy adhesives for use in bonding many metals, wood, and a variety of plastics. Equal parts by volume are easily mixed to produce strong, impact-resistant bonds.Information provided by 3M
Physical Properties Metric English Comments
Brookfield Viscosity >= 1.00e+6 cP
>= 1.00e+6 cP
RVF, #7 spindle, 2 rpm at RT
Mechanical Properties Metric English Comments
Hardness, Shore D 75 - 80
75 - 80
Shear Strength 2.76 MPa
400 psi
Overlap on Etched Aluminum, cured for 20 mins @ RT; ASTM D1002
3.45 MPa
500 psi
Overlap on Etched Aluminum, cured for 30 mins @ RT; ASTM D1002
5.17 MPa
750 psi
Overlap on Etched Aluminum, cured for 60 mins @ RT; ASTM D1002
6.21 MPa
900 psi
Overlap on Etched Aluminum, cured for 90 mins @ RT; ASTM D1002
12.5 MPa
1810 psi
Overlap on Etched Aluminum, Tap Water @ RT for 14 days; ASTM D1002
13.07 MPa
1895 psi
Overlap on Etched Aluminum, Salt Spray @ 35°C for 14 days; ASTM D1002
14.0 MPa
2030 psi
Overlap on Etched Aluminum, 100% RH @ 49°C for 14 days; ASTM D1002
1.03 MPa

@Temperature 82.0 °C
150 psi

@Temperature 180 °F
Steel Overlap; ASTM D1002
2.07 MPa

@Temperature 82.0 °C
300 psi

@Temperature 180 °F
Aluminum Overlap; ASTM D1002
6.89 MPa

@Temperature -55.0 °C
1000 psi

@Temperature -67.0 °F
Steel Overlap; ASTM D1002
10.3 MPa

@Temperature -55.0 °C
1500 psi

@Temperature -67.0 °F
Aluminum Overlap; ASTM D1002
13.8 MPa

@Temperature 24.0 °C
2000 psi

@Temperature 75.2 °F
Steel Overlap; ASTM D1002
16.5 MPa

@Temperature 24.0 °C
2400 psi

@Temperature 75.2 °F
Aluminum Overlap; ASTM D1002
Peel Strength 0.701 kN/m
4.00 pli
Aluminum T-Peel; ASTM D1876
1.75 kN/m
10.0 pli
Steel T-Peel; ASTM D1876
Thermal Properties Metric English Comments
CTE, linear 60.0 µm/m-°C

@Temperature -50.0 - 10.0 °C
33.3 µin/in-°F

@Temperature -58.0 - 50.0 °F
234 µm/m-°C

@Temperature 50.0 - 110 °C
130 µin/in-°F

@Temperature 122 - 230 °F
Thermal Conductivity 0.334 W/m-K
2.32 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+13 ohm-cm
1.20e+13 ohm-cm
Dielectric Strength 27.6 kV/mm
700 kV/in
Descriptive Properties Value Comments
Appearance Black
Accelerator
Gray
White
Base
Users viewing this material also viewed the following: