Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
ASTM C158
Rogers Corporation Bisco™ HT-870 Cellular Silicone Foam
Gasketing and sealing rating is JMLU-2 (Listed) per UL 157. No UV degradation per SAE J-1960. Ozone effect rating is 0 (no cracks) per ASTM D-1171. No staining per ASTM D-925(A). Passes AMS-3568..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® D02 PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® D02TS PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® D03 PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® D05 PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® DET PFPE Fluid
Galden® D grades are specifically recommended for electronic reliability testing, including thermal shock and hermetic seal testing.Galden® PFPE is a line of high-performance, inert, fluorinat..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® HS240 PFPE VPS Fluid
Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® HS260 PFPE VPS Fluid
Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® LLS215 PFPE VPS Fluid
Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® LS200 PFPE VPS Fluid
Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Solvay Specialty Polymers Galden® LS230 PFPE VPS Fluid
Galden® LS and HS grades are specifically recommended for vapor phase soldering.Galden® PFPE is a line of high-performance, inert, fluorinated fluids. Various grades, with a variety of servic..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Elisto THERMOSTAR® XPS Mold Insulation Material
Lateral insulationInformation provided by elisto
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
Liquid
3M Fluorinert™ FC-70 Electronic Liquid
Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a..
Thermal Conductivity 0.0700 W/m-K
0.486 BTU-in/hr-ft²-°F
3M K20 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..