Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.645 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.645 W/m-K
4.48 BTU-in/hr-ft²-°F
Arlon AR1000 Glass, PTFE and Micro-Dispersed Ceramic
Used in the RF and microwave industries.Information provided by Arlon Materials for Electronics (MED).
Copyright © lookpolymers.com All Rights Reserved