Polymer Property : Thermal Conductivity = 0.770 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.770 W/m-K
5.34 BTU-in/hr-ft²-°F
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data)
Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig..
Thermal Conductivity 0.770 W/m-K
5.34 BTU-in/hr-ft²-°F
Schott LAFN7 Glass
Information Provided by SCHOTT North America, Inc.