Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.770 W/m-K | 5.34 BTU-in/hr-ft²-°F | |
Quadrant EPP Fluorosint® 500 PTFE + mica, compression moulded (ISO Data) Reinforced with a proprietary synthetic mica, this material exhibits, in addition to its inherent outstanding chemical and hydrolysis resistance, very good mechanical and tribological properties Hig.. |
|||
Thermal Conductivity | 0.770 W/m-K | 5.34 BTU-in/hr-ft²-°F | |
Schott LAFN7 Glass Information Provided by SCHOTT North America, Inc. |