Thermal Properties Metric English Comments
Thermal Conductivity 1.15 - 1.30 W/m-K
8.00 - 9.00 BTU-in/hr-ft²-°F
Master Bond EP76M-F Electrically Conductive, Two Part Epoxy
Description: Master Bond EP76M-F is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing, and coating formulated to cure at room temperature or ..
Thermal Conductivity 1.15 - 1.30 W/m-K
8.00 - 9.00 BTU-in/hr-ft²-°F
Master Bond MasterSil 156 Two Part, Low Viscosity Silicone
Description: Master Bond MasterSil 156 is a two component, lower viscosity silicone system for high performance potting, encapsulation and sealing. MasterSil 156 combines high temperature resistance..