Polymer Property : Thermal Conductivity = 1.35 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 1.35 W/m-K

@Temperature 538 °C
9.37 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Pyrotek Pyrethrum FA 800 Woven Stainless Steel Fabric
Pyrotherm FA 800 is a durable, heat-resistant woven fabric made from 316L stainless steel fibers. The fabric maintains its mechanical strength and cloth-like softness in high temperature, abrasive ..
Thermal Conductivity 1.35 W/m-K
9.37 BTU-in/hr-ft²-°F
Mateck Fused Silica IR Grade (SiO2)
Optical crystals
Thermal Conductivity 1.35 W/m-K

@Temperature 20.0 °C
9.37 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Mateck Fused Silica UV-VIS Grade (SiO2)
Optical crystals
Thermal Conductivity 1.35 W/m-K
9.37 BTU-in/hr-ft²-°F
UBE Tyranno Grade LoxM Ceramic High Temperature Fiber
Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e..
Thermal Conductivity 1.35 W/m-K
9.37 BTU-in/hr-ft²-°F
Product Property; ASTM E 1530
Arlon Thermabond® T20 (99710W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: 8 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Prim..