Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.54 W/m-K @Temperature 100 °C |
10.7 BTU-in/hr-ft²-°F @Temperature 212 °F |
overall; Arlon SQA-TMS-054 |
Arlon R37806X030 Silicone Rubber/Fiberglass Interleave: 3 mil PE; Side 2: uncured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |