Thermal Properties Metric English Comments
Thermal Conductivity 1.65 W/m-K
11.5 BTU-in/hr-ft²-°F
Loctite® 3873 1 component acrylic High Conductivity Flexible Adhesive
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..
Thermal Conductivity 1.65 W/m-K
11.5 BTU-in/hr-ft²-°F
in plane; ASTM E1461
DSM Arnite® AV2 370 XL-T PET-GF35
35% Glass Reinforced, Low Outgassing, Thermal conductive material