Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 16.7 W/m-K | 116 BTU-in/hr-ft²-°F | |
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The a.. |
|||
Thermal Conductivity | 16.7 W/m-K | 116 BTU-in/hr-ft²-°F | |
Special Metals NILO® Alloy K Controlled-Expansion Alloy Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat.. |
|||
Thermal Conductivity | 16.7 W/m-K | 116 BTU-in/hr-ft²-°F | ASTM C408 |
CoorsTek AD-90 Alumina (nom. 90% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
Thermal Conductivity | 16.7 W/m-K | 116 BTU-in/hr-ft²-°F | test temperature unknown |
Special Metals INCOLOY® Alloy 903 A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a.. |