Polymer Property : Thermal Conductivity = 16.7 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 16.7 W/m-K
116 BTU-in/hr-ft²-°F
Special Metals NILO® Alloy 48 Controlled-Expansion Alloy
Inflection point 460°C. A nickel-iron controlled-expansion alloy containing 48% nickel. Its coefficient of thermal expansion is designed to match that of soft lead and soda-lime glasses. The a..
Thermal Conductivity 16.7 W/m-K
116 BTU-in/hr-ft²-°F
Special Metals NILO® Alloy K Controlled-Expansion Alloy
Inflection point 450°C. A nickel-iron-cobalt controlled-expansion alloy containing 29% nickel. Its coefficient of expansion, which decreases with rising temperature to the inflection point, mat..
Thermal Conductivity 16.7 W/m-K
116 BTU-in/hr-ft²-°F
ASTM C408
CoorsTek AD-90 Alumina (nom. 90% Al2O3)
Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Thermal Conductivity 16.7 W/m-K
116 BTU-in/hr-ft²-°F
test temperature unknown
Special Metals INCOLOY® Alloy 903
A nickel-iron-cobalt alloy with additions of niobium, titanium, and aluminum for precipitation hardening. The alloy combines high strength with a low and constant coefficient of thermal expansion a..