Polymer Property : Thermal Conductivity = 12.1 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 12.1 W/m-K

@Temperature 100 °C
84.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 0% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 12.1 W/m-K

@Temperature 100 °C
84.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 10% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 12.1 W/m-K

@Temperature 100 °C
84.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 20% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 12.1 W/m-K

@Temperature 100 °C
84.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 12.1 W/m-K

@Temperature 100 °C
84.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 30% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 12.1 W/m-K

@Temperature 100 °C
84.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 40% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 12.1 W/m-K

@Temperature 100 °C
84.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, 50% cold work
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ..
Thermal Conductivity 12.1 W/m-K
84.0 BTU-in/hr-ft²-°F
SGL Carbon Group EK 20 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Thermal Conductivity 12.1 W/m-K
84.0 BTU-in/hr-ft²-°F
Special Metals NI-SPAN-C® Alloy 902
A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo..
Thermal Conductivity 12.1 W/m-K
84.0 BTU-in/hr-ft²-°F
Special Metals UDIMET® alloy 188 Cobalt-base Alloy
UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small ..
Thermal Conductivity 12.1 W/m-K

@Temperature 100 °C
84.0 BTU-in/hr-ft²-°F

@Temperature 212 °F
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched
The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea..
Copyright © lookpolymers.com All Rights Reserved