Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 12.1 W/m-K @Temperature 100 °C |
84.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® B-3® alloy, 0% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 12.1 W/m-K @Temperature 100 °C |
84.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® B-3® alloy, 10% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 12.1 W/m-K @Temperature 100 °C |
84.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® B-3® alloy, 20% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 12.1 W/m-K @Temperature 100 °C |
84.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® B-3® alloy, 3.2 mm bright annealed sheet The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 12.1 W/m-K @Temperature 100 °C |
84.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® B-3® alloy, 30% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 12.1 W/m-K @Temperature 100 °C |
84.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® B-3® alloy, 40% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 12.1 W/m-K @Temperature 100 °C |
84.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® B-3® alloy, 50% cold work The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and .. |
|||
Thermal Conductivity | 12.1 W/m-K | 84.0 BTU-in/hr-ft²-°F | |
SGL Carbon Group EK 20 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Thermal Conductivity | 12.1 W/m-K | 84.0 BTU-in/hr-ft²-°F | |
Special Metals NI-SPAN-C® Alloy 902 A nickel-iron-chromium alloy made precipitation hardenable by additions of aluminum and titanium. The titanium content also helps provide a controllable thermoelastic coefficient, which is the allo.. |
|||
Thermal Conductivity | 12.1 W/m-K | 84.0 BTU-in/hr-ft²-°F | |
Special Metals UDIMET® alloy 188 Cobalt-base Alloy UDIMET® alloy 188 (UNS R30188) is a cobalt-base alloy with excellent high-temperature strength and good oxidation resistance to 2000°F (1093°C). The high chromium level coupled with small .. |
|||
Thermal Conductivity | 12.1 W/m-K @Temperature 100 °C |
84.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes Hastelloy® B-3® alloy, heat treated at 1065°C, rapid quenched The attributes of Corrosion-Resistant HASTELLOY® alloys include high resistance to uniform attack, outstanding localized corrosion resistance, excellent stress corrosion cracking resistance, and ea.. |