Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Cold Drawn High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, Hydrogen Annealed at 2150°F (1177°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Cold-Rolled High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Strip, Formed and Deep Draw Quality High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | c direction |
MarkeTech Rutile (TiO2) Fiber Optic Crystal More chemically and physically resistant than Yttrium Vanadate. Large birefringence. Used for fiber optic beam displacers and optical isolators. Grown by Vernull method. Transmission range 500 to.. |
|||
Thermal Conductivity | 13.0 W/m-K @Temperature 20.0 °C |
90.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel SIRIUS 800 H+ Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
Thermal Conductivity | 13.0 W/m-K @Temperature 20.0 °C |
90.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel URANUS® B25 6 Mo Cost Saving Super-Austenitic Stainless Steel with PREN = 42 Description: URANUS® B25 (UR B25) is a 18% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed to be cost effective. The 18% nickel and 0... |
|||
Thermal Conductivity | 13.0 W/m-K @Temperature 20.0 °C |
90.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43 Description: URANUS® B26 (UR B26) is a 25% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed for high structural stability and high corr.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
Momentive Performance Materials Niobium Carbide (NbC) Coating High temperature protective coating for graphite.TaC, NbC, and ZrC coatings resist chemical attack by corrosive liquids and gases at very high temperatures. They are finding increasing acceptance i.. |
|||
Thermal Conductivity | 13.0 W/m-K @Temperature 20.0 °C |
90.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel SIRIUS 800 Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
Thermal Conductivity | 13.0 W/m-K @Temperature 100 °C |
90.2 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Haynes 263® alloy, cold rolled sheet, solution treated and aged Very good aged strength properties, excellent fabrication characteristics when annealed, excellent intermediate temperature tensile ductility, is not normally subject to strain age cracking, excelle.. |
|||
Thermal Conductivity | 13.0 W/m-K @Temperature 100 °C |
90.0 BTU-in/hr-ft²-°F @Temperature 212 °F |
|
Schmolz + Bickenbach MoldMAX LH® Low Hard - Copper Alloy Description: Brush Wellman’s MoldMAX LH® (Low Hard) is a premium copper mold alloy that provides hardness and strength comparable with standard AISI P-20 tool steel and a thermal conductivit.. |
|||
Thermal Conductivity | 13.0 W/m-K @Temperature 20.0 - 100 °C |
90.2 BTU-in/hr-ft²-°F @Temperature 68.0 - 212 °F |
|
CeramTec Ziralit Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 CeramTec's Zirconia Toughened Alumina (Ziralit) provides excellent strength, excellent temperature performance, and superior toughness. It has enhanced performance for high quantity volume productio.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | ASTM C408 |
CoorsTek Alumina-Zirconia Composite, AZ-25 Information provided by CoorsTek. |
|||
Thermal Conductivity | 13.0 - 14.6 W/m-K | 90.2 - 101 BTU-in/hr-ft²-°F | as built, XY direction |
EOS PH1 Precipitation Hardening Stainless Steel for DMLS 3D Printing EOS Stainless Steel PH1 is a stainless steel powder which has been optimized especially for processing on EOSINT M 270 systems. This stainless steel prototyping material is tough and resistant to .. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
California Fine Wire Stablohm 610 Nickel, Chromium and Iron Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.0 BTU-in/hr-ft²-°F | |
Atom Adhesives AA-DUCT 906 Epoxy Adhesive AA-DUCT 906 represents the newest technology since the introduction of electrically conductive silver compounds. This unique formulation is based on a silver coated ceramic that results in lower mat.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
Resistalloy International Resistalloy 3718 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
Resistalloy International Resistalloy 6015 Nickel Chromium Electrical Resistance Alloy Used mainly for electrical elements in both industrial and domestic applications. Industrial applications vary from small laboratory kilns to heavy-duty heat-treatment furnaces under all types of at.. |
|||
Thermal Conductivity | 13.0 W/m-K @Temperature 20.0 °C |
90.2 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel SIRIUS 800 H Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at tempe.. |
|||
Thermal Conductivity | 13.0 W/m-K @Temperature 85.0 °C |
90.2 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy 39 Bismuth Solder Alloy Low temperature eutectic solder. Can be used on the same metallization as SnPb based solders. Lowest temperature solder pasteInformation Provided by Indium Corporation |
|||
Thermal Conductivity | 13.0 W/m-K | 90.2 BTU-in/hr-ft²-°F | |
High Temp Metals Alloy 49 Iron-Nickel High Permeability Alloy, Bar, After Process Annealed at 1600°F (871°C) High Permeability "49" alloy is a 48% nickel-iron alloy which has a saturation flux density of approximately 15,000 Gauss after hydrogen annealing. Hysteresis loss is very low in either DC or AC cir.. |