Thermal Properties Metric English Comments
Thermal Conductivity 14.26 W/m-K
98.96 BTU-in/hr-ft²-°F
Special Metals INCONEL® Alloy MA 754
A mechanically alloyed nickel-chromium alloy with oxide dispersion strengthening. Mechanical alloying, which involves high-energy milling of metal powders, is used to create a uniformly distributed..