Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 156 W/m-K @Temperature 15.6 °C |
1080 BTU-in/hr-ft²-°F @Temperature 60.0 °F |
|
Performance Alloys MoldStar® 90 Copper Mold Alloy Description: MoldStar® 90 is a beryllium-free copper alloy for the blow molding and injection molding industries as well as other industrial applications. MoldStar® 90 provides a good balance of t.. |