Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 165 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Misumi DC53 JIS Tool Steel
General purpose cold work die and mold steel whose strength and toughness approach those of high speed steels. Good machinability and grindability. Tougher than D2 Tool Steel. Machines 30% faster th..
Thermal Conductivity 23.8 W/m-K

@Temperature 800 °C
165 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-120® alloy, solution heat-treated
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 23.8 W/m-K

@Temperature 800 °C
165 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 23.8 W/m-K

@Temperature 800 °C
165 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 23.8 W/m-K

@Temperature 800 °C
165 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 23.8 W/m-K

@Temperature 800 °C
165 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours
Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts ..
Thermal Conductivity 23.8 W/m-K

@Temperature 800 °C
165 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Haynes 718 alloy, cold rolled, solution-treated and aged sheet
Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar
Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Strip
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Annealed and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 or..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Wire
Tensile strength (ultimate) and elongation values reported here are typical for Annealed and Aged Wire specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy i..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Age Hardened
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar
Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed Rod and Bar specifically. Other property values are typical of ann..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Age Hardened
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 3..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Age Hardened
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Wire
Tensile strength (ultimate) and elongation values reported here are typical for Annealed Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gen..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar
Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Cold-Drawn and Aged Rod and Bar specifically. Other property values are typ..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Age Hardened
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn Rod and Bar
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Cold-Drawn Rod and Bar specifically. Other property values are typical of annealed DURANICKEL®..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard and Aged Strip
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 o..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Age Hardened
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard Strip
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Age Hardened
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished Rod and Bar
Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished Rod and Bar specifically. Other property values are typical of annealed DURANICKELÂ..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Age Hardened
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the al..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the ..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Age Hardened
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire
Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gener..
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire, Aged
Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy in gen..
Copyright © lookpolymers.com All Rights Reserved