Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard Strip

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name DURANICKEL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard Strip.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in general.Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.19 g/cc
0.296 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell C 25 - 34
25 - 34
Tensile Strength, Ultimate 896 - 1070 MPa
130000 - 155000 psi
Elongation at Break 3.0 - 15 %
3.0 - 15 %
Modulus of Elasticity 207 GPa
30000 ksi
Tension
Poissons Ratio 0.31
0.31
Shear Modulus 76.0 GPa
11000 ksi
Thermal Properties Metric English Comments
CTE, linear 13.0 µm/m-°C

@Temperature 21.0 - 100 °C
7.22 µin/in-°F

@Temperature 69.8 - 212 °F
Mean; aged
14.0 µm/m-°C

@Temperature 21.0 - 300 °C
7.78 µin/in-°F

@Temperature 69.8 - 572 °F
Mean; aged
14.7 µm/m-°C

@Temperature 21.0 - 500 °C
8.17 µin/in-°F

@Temperature 69.8 - 932 °F
Mean; aged
16.6 µm/m-°C

@Temperature 21.0 - 900 °C
9.22 µin/in-°F

@Temperature 69.8 - 1650 °F
Mean; aged
Specific Heat Capacity 0.435 J/g-°C

@Temperature 20.0 - 100 °C
0.104 BTU/lb-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 23.8 W/m-K
165 BTU-in/hr-ft²-°F
Age Hardened
Melting Point 1400 - 1440 °C
2550 - 2620 °F
Solidus 1400 °C
2550 °F
Liquidus 1440 °C
2620 °F
Component Elements Properties Metric English Comments
Aluminum, Al 4.0 - 4.75 %
4.0 - 4.75 %
Carbon, C <= 0.30 %
<= 0.30 %
Copper, Cu <= 0.25 %
<= 0.25 %
Iron, Fe <= 0.60 %
<= 0.60 %
Manganese, Mn <= 0.50 %
<= 0.50 %
Nickel, Ni >= 93 %
>= 93 %
Including Cobalt
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.010 %
<= 0.010 %
Titanium, Ti 0.25 - 1.0 %
0.25 - 1.0 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000424 ohm-cm
0.0000424 ohm-cm
Aged
Curie Temperature 15.0 - 50.0 °C
59.0 - 122 °F