Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 165.01 W/m-K | 1145.1 BTU-in/hr-ft²-°F | |
ALIMEX AMP 8000 Aluminum Plate AMP 8000 offers higher strength levels, good machinability and dimensional stability. Its tensile strength is up to 40% higher than AlZn5.5MgCu (7075). Moulding, (Prototypes) injection moulds, Jig .. |