Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 140 - 170 W/m-K | 972 - 1180 BTU-in/hr-ft²-°F | |
MarkeTech AN 160 Aluminum Nitride Ceramic Substrate, 99% Purity Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 5.5 x 3.6 in. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 µ.. |
|||
Thermal Conductivity | 165 - 170 W/m-K | 1150 - 1180 BTU-in/hr-ft²-°F | z direction |
MarkeTech Cu/Mo/Cu 1:5:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Thermal Conductivity | 160 - 170 W/m-K | 1110 - 1180 BTU-in/hr-ft²-°F | z direction |
MarkeTech Cu/Mo/Cu 13:74:13 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Thermal Conductivity | 150 - 170 W/m-K | 1040 - 1180 BTU-in/hr-ft²-°F | Temper T651 |
Constellium PLAN 6061 Aluminum Rolled Plate Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Thermal Conductivity | 150 - 170 W/m-K | 1040 - 1180 BTU-in/hr-ft²-°F | Temper T651 |
Constellium PLAN 6082 Aluminum Rolled Plate Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv.. |
|||
Thermal Conductivity | 150 - 170 W/m-K | 1040 - 1180 BTU-in/hr-ft²-°F | temper T651 |
Constellium Planoxal® 60 Aluminum plate The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use.. |
|||
Thermal Conductivity | 150 - 170 W/m-K | 1040 - 1180 BTU-in/hr-ft²-°F | Temper T651 |
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |
|||
Thermal Conductivity | 150 - 170 W/m-K | 1040 - 1180 BTU-in/hr-ft²-°F | Temper T651 |
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta.. |