Polymer Property : Thermal Conductivity = 150 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 150 W/m-K

@Temperature 0.000 - 100 °C
1040 BTU-in/hr-ft²-°F

@Temperature 32.0 - 212 °F
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar
Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part..
Thermal Conductivity 150 W/m-K

@Temperature 0.000 - 100 °C
1040 BTU-in/hr-ft²-°F

@Temperature 32.0 - 212 °F
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate
Aluminium alloy 2124 reinforced with 25 volume % silicon carbide particles (average size 3 micron). It is manufactured by a powder metallurgy route using high-energy mixing to ensure excellent part..
Thermal Conductivity 150 - 240 W/m-K
1040 - 1670 BTU-in/hr-ft²-°F
H.C. Starck WCu 70/30 Tungsten-Copper Composite Material
Description of Product: Tungsten-copper composite materials are produced by copper infiltration of porous sintered tungsten. They are available with different copper contents (10 - 30 %). A therm..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
In-Plane; Angstrom's Method
GrafTech eGRAF® HITHERM™ HT-1205 Graphite
Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
In-Plane; Angstrom's Method
GrafTech eGRAF® HITHERM™ HT-1210 Graphite
Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
In-Plane; Angstrom's Method
GrafTech eGRAF® HITHERM™ HT-1220 Graphite
Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
Specialty Materials SCS-6 Silicon Carbide Monofilament
High strength at high temperature. These fibers are used in metal, ceramic and polymer matrix composites and are extremely effective for high-temperature applications. Silicon carbide reinforced tit..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
ASTM E1461
M Cubed Technologies SSC-FG Reaction-Bonded Silicon Carbide, Fine-Grained
Fine-grained reaction-bonded SiC. Used for mechanical seals and other SiC applications that require a high surface finish/tight tolerances. Si content can be tailored for the application.Informati..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
UCAR Carbon UCAR® CBY Extruded Graphite
Grade CBY is a general purpose, cost effective extruded graphite with improved strength, structure and density characteristics. It is a low ash graphite for superior oxidation resistance.Typical App..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
UCAR Carbon UCAR® CHV Extruded Graphite
Typical uses for extruded grades are in the production of molds and crucibles, heating elements and furnace furniture, liquid metal processing equipment and chemical process equipment.Tabular proper..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
Constellium Certal® SPC Aluminum
Certal® SPC has been optimized to provide excellent machinability, good shape stability and high strength properties throughout the plate thickness. Uniform strength is an important property in man..
Thermal Conductivity 150 - 170 W/m-K
1040 - 1180 BTU-in/hr-ft²-°F
Temper T651
Constellium PLAN 6061 Aluminum Rolled Plate
Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Thermal Conductivity 150 - 170 W/m-K
1040 - 1180 BTU-in/hr-ft²-°F
Temper T651
Constellium PLAN 6082 Aluminum Rolled Plate
Rolled plates in 6082 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6082 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Thermal Conductivity 150 - 170 W/m-K
1040 - 1180 BTU-in/hr-ft²-°F
temper T651
Constellium Planoxal® 60 Aluminum plate
The advantage of Planoxal®-60 plates over other standard EN AW-6082 alloy products is their low level of internal stress. They are also suitable for technical anodizing. Planoxal®-60 is mainly use..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
ASTM C408
CoorsTek Direct Sintered Silicon Carbide, SC DS (SC-30, UltraSiC™)
Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
CRP Technology 8601 Aerospace Grade Power Metallurgy Aluminum Alloy
For Motorsport and Aerospace marketplaces: manufactured by a special powder metallurgy process using a high-energy mixing process which ensures excellent mechanical properties.Super Aluminium materi..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition
AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route us..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
CMW® ELKONITE® 10W53 Heat Treatable Copper Tungsten
Uses: Resistance / projection welding electrodesInformation provided by CMW Inc.
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
CMW® ELKONITE® 1W3 Copper Tungsten RWMA Class 10
Uses: Arcing and current carrying electrical contacts. Resistance/projection welding electrodes.Information provided by CMW Inc.
Thermal Conductivity 150 - 170 W/m-K
1040 - 1180 BTU-in/hr-ft²-°F
Temper T651
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
Thermal Conductivity 150 - 170 W/m-K
1040 - 1180 BTU-in/hr-ft²-°F
Temper T651
Constellium ALPLAN® 6082 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6082 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..
Thermal Conductivity 150 W/m-K
1040 BTU-in/hr-ft²-°F
ASTM E1461
M Cubed Technologies ASC-301 Aluminum alloy-30% SiC Metal Matrix Composite
High stiffness, low density composite. Parts are cast using several standard foundry techniques Size range varies from small components (1lb or smaller) to parts greater than 10 ft. square with co..