Polymer Property : Thermal Conductivity = 180 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 170 - 180 W/m-K
1180 - 1250 BTU-in/hr-ft²-°F
z direction
MarkeTech Cu/Mo/Cu 1:4:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
Thermal Conductivity 170 - 180 W/m-K
1180 - 1250 BTU-in/hr-ft²-°F
z direction
MarkeTech Cu/Mo70-Cu30/Cu 1:4:1 Laminated Sheet
Cu/Mo/Cu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated he..
Thermal Conductivity 170 - 180 W/m-K
1180 - 1250 BTU-in/hr-ft²-°F
MarkeTech WCu10 Tungsten Copper Alloy
Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st..