Polymer Property : Thermal Conductivity = 180.44 BTU-in/hr-ft²-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 26.001 W/m-K
180.44 BTU-in/hr-ft²-°F
Latrobe LSSâ„¢ A2 Tool Steel (ASTM A2)
TLS A2 tool steel is a versatile, air-hardening tool steel that is characterized by good toughness and excellent dimensional stability in heat treatment. TLS A2 is intermediate in wear resistance be..